Search
Now showing items 1-10 of 32
Structures of Ni - Ni Nan contacts obtained by the electrode position in the presence of a magnetic field / Struktura nikal - nikal nanokontakta dobijenih elektrohemijskim taloženjem
(Belgrade, Serbia : Engineering Society for Corrosion, 2005)
Structures of Ni - Ni Nan contacts obtained by the electrode position at the different cathodic potentials were analyzed. Ni - Ni Nan contacts were electrodeposited from a Watt solution in the presence of coumarone, and ...
Corrosion of chromium white cast iron in acidic medium / Korozija visokohromnog belog gvožđa u kiseloj sredini
(Belgrade, Serbia : Engineering Society for Corrosion, 2008)
In this work we studied the electrochemical behavior of chromium white cast irons in deaerated aqueous sulphuric acid solutions of the pH 1-3. The measurements of concentrations of dissolved iron and chromium in the solution, ...
Analysis of morphologies of magnetic nanocontacts obtained by electrochemical deposition and their magnetoresistance / Analiza morfologija elektrohemijski dobijenih magnetnih nanokontakta i njihova magnetorezistencija
(Belgrade, Serbia : Engineering Society for Corrosion, 2005)
In this work, morphologies of Fe - Fe, Co - Co and Ni81Fel9 – Ni81Fe19 nanocontacts obtained by the electrode position were analyzed. The obtained nanocontacts showed a very large ballistic magnetoresistance. It was shown ...
The roughness analysis of metal coatings by STM technique: Part II: Analysis of zinc coatings / Analiza hrapavosti galvanskih prevlaka tehnikom skenirajuće tunelske mikroskopije - deo II - analiza prevlaka cinka
(Belgrade, Serbia : Engineering Society for Corrosion, 2002)
In this work is given the analysis of roughness of zinc coatings electrodeposited from a sulfate bath in the presence of dextrin and 2-hidroxi-benzaldehyde, by methodology which is described in part I of this work. It was ...
The roughness analysis of metal coatings by STM technique: Part I: Theoretical survey / Analiza hrapavosti galvanskih prevlaka tehnikom skenirajuće tunelske mikroskopije - deo I - teorijski osnovi
(Belgrade, Serbia : Engineering Society for Corrosion, 2002)
In this work is given theoretical base of methodology which, by use STM technique and corresponding STM software, offers an good conveniences for the examination of mechanism of electrode position process.
Characterization of electrochemically synthesized pani on graphite electrode for potential use in electrochemical power sources / Elektrohemijska sinteza i karakterizacija elektrode od polianilina za potencijalnu upotrebu u elektrohemijskim izvorima energije
(Belgrade, Serbia : Engineering Society for Corrosion, 2009)
Polyaniline (PANI) on graphite electrode was synthesized electrochemically under galvanostatic condition at current density of 2.0 mA cm-2 from aqueous solution of 1.0 moldm-3 HCl and 0.25 mol dm-3 aniline monomer. ...
Influence of the structure of metallic chromium on its electrochemical and chemical corrosion / Uticaj strukture metalnog hroma na njegovu elektrohemijsku i hemijsku koroziju
(Belgrade, Serbia : Engineering Society for Corrosion, 2005)
It was shown that metallic chromium in aqueous solution of sulfuric acid dissolves in accord with the electrochemical mechanism proposed by Wagner and Traud, but also by a direct chemical reaction of metal with water ...
Activated titanium anodes in cathodic protection: A comparison of the characteristics of anodes prepared by sol-gel procedure and thermal decomposition / Aktivirane titanske anode u katodnoj zaštiti - poređenje karakteristika anoda dobijenih sol-gel postupkom i termičkom razgradnjom
(Belgrade, Serbia : Engineering Society for Corrosion, 2004)
Polarization characteristics of titanium anodes, coated by active RuO2-TiO2 binary oxide using sol-gel preparation procedure and chloride thermal decomposition, in oxygen evolution reaction during anode electrolytic ...
New method of Ni/WC and Cu/WC composite coatings formation / Novi način formiranja kompozitnih prevlaka
(Belgrade, Serbia : Engineering Society for Corrosion, 2004)
Ni/WC and Cu/WC composite coatings were obtained in two steps. The first step consists of the inert WC particles deposition from the aqueous solution onto steel surface by means of a micro-pipette and covering by the dilute ...
Kinetic of corrosion reactions in acid and neutral solutions on electrochemically deposited Ni-W alloys / Kinetika korozionih reakcija u kiselim i neutralnim rastvorima na elektrohemijski taloženim legurama Ni-W
(Belgrade, Serbia : Engineering Society for Corrosion, 2006)
Ni-W alloys were electrochemically deposited from an ammonia-citrate electrolyte on rotating disc electrode with a gold disc, by direct and pulsating current. The corrosion potential and kinetics of cathodic and anodic ...