Methanol electrooxidation on PtRu modified zeolite X
(International Institute for the Science of Sintering, Beograd, 2013)
Zeolite NaX (faujasite type) was used as a support for platinum-ruthenium catalyst. A procedure for thermal decomposition of noble metal acetylacetonates to deposit noble metal clusters on the surface of solid support was ...
Cyclic Voltammetric Study of the Influence of Porosity on Electrochemical Response of Nickel-Alumina Modified Glassy Carbon Electrode
(International Institute for the Science of Sintering, Beograd, 2018)
Pure and nickel-modified alumina powders with different porosity were synthesized and applied on the glassy carbon electrode by means of Nafion polymer. The data obtained from the nitrogen adsorption-desorption isotherm ...
Study of Nd-Fe-B alloys with nonstoichiometric Nd content in optimal magnetic state
(International Institute for the Science of Sintering, Beograd, 2009)
Characterization of two rapid-quenched Nd-Fe-B alloys with nonstoichiometric Nd content in the optimized magnetic state was carried out using the X-ray diffractometry (XRD), 57Fe Mössbauer spectroscopic phase analysis (MS), ...
A comparative thermomagnetic study of melt-spun Nd-Fe-B alloys with different Nd content
(International Institute for the Science of Sintering, Beograd, 2009)
Changes in the phase composition and magnetic properties of three types of commercial Nd-Fe-B alloys with different Nd content - low (10-12 wt%), near stoichiometric (21-25 wt%) and rich (26-29 wt%) caused by thermomagnetic ...
Anisotropy Analysis of Low Cement Concrete by Ultrasonic Measurements and Image Analysis
(International Institute for the Science of Sintering, Beograd, 2016)
The analized material was high alumina low cement castable sintered at three different temperatures. Influence of initial material anisotropy on the thermal shock resistance as well as changes of anisotropy level during ...
The Effect of Sintering Temperature on Mesoporous Structure of WO3 Doped Tio(2) Powders
(International Institute for the Science of Sintering, Beograd, 2018)
In this study, WO3 doped TiO2 powders were synthesized via sol-gel method combined with a hydrothermal process. The effect of sintering temperature on mesoporous structure and catalytic activities of these powders were ...
Microstructure refinement and physical properties of Ag-SnO2 based contact materials prepared by high-energy ball milling
(International Institute for the Science of Sintering, Beograd, 2013)
High energy ball milling was used in order to improve dispersion of metal oxide in Ag-SnO2 electrical contact materials. The processed Ag-SnO2 (92:8) and Ag-SnO2In2O3 (87.8:9.30:2.9) powder mixtures were subsequently ...
Organobentonite: Characterization and Adsorptive Properties towards Phenol and its Derivatives
(International Institute for the Science of Sintering, Beograd, 2016)
Bentonite from Mecji Do locality in Serbia was modified with hexadecyltrimethylammonium bromide (HDTMA-Br), and the sample was denoted as HDTMA-MD. The characterization of the material included X-Ray diffraction, elemental ...
Mechanical Properties of Biomass-derived Silica Nanoparticles Reinforced PMMA Composite Material
(Science of Sintering, 2022)
Rice husk was used to produce silica particles, which were then used to reinforce the polymer matrix. The synthesized SiO2 particles were characterized using X-ray diffraction, Fourier transforms infrared spectroscopy ...
Effect of Sintering Temperature and Calcium amount on Compressive Strength of Brushite-Metakaolin Polymer Materials
(Association for ETRAN Society, 2022)
The effect of Ca2+ amount and sintering temperature on mechanical properties of geopolymer-brushite (GPB) binders was investigated. Brushite and raw abandoned kaolinite clay thermally transformed into metakaolin were used ...