Electrocrystallization of silver dendrites / Elektrokristalizacija dendrita srebra
(Belgrade, Serbia : Engineering Society for Corrosion, 2014)
Morphology of electrodeposited silver dendrites was investigated by scanning electron microscope (SEM). On the basis of morphological analysis, the structures and mechanism of growth were proposed. Silver dendrite is twin ...
Electrochemical deposition of powder alloy Co-Ni-Mo-O / Elektrohemijsko dobijanje prahova legure Co-Ni-Mo-O
(Belgrade, Serbia : Engineering Society for Corrosion, 2008)
The electro deposition of the Co-Ni-Mo-O alloy powders from alkaline ammonium electrolytes and at constant current density was investigated. Metals of iron group, Co and Ni induce deposition of Mo, which alone can not be ...
The kinetics of passivation based on the reduction of current density under potentiostatic conditions for a martensitic stainless steel / Kinetika pasivizacije bazirane na redukciji gustine struje pri potenciostatskim uslovima za martenzitni nerđajući čelik
(Belgrade, Serbia : Engineering Society for Corrosion, 2016)
The potentiostatic method and the theory of 'topochemical reactions' in the kinetics of the active dissolution and passivation process of AISI 420 stainless steel were studied. It was found that, to a great extent, the ...
Analysis of morphologies of magnetic nanocontacts obtained by electrochemical deposition and their magnetoresistance / Analiza morfologija elektrohemijski dobijenih magnetnih nanokontakta i njihova magnetorezistencija
(Belgrade, Serbia : Engineering Society for Corrosion, 2005)
In this work, morphologies of Fe - Fe, Co - Co and Ni81Fel9 – Ni81Fe19 nanocontacts obtained by the electrode position were analyzed. The obtained nanocontacts showed a very large ballistic magnetoresistance. It was shown ...
The roughness analysis of metal coatings by STM technique: Part I: Theoretical survey / Analiza hrapavosti galvanskih prevlaka tehnikom skenirajuće tunelske mikroskopije - deo I - teorijski osnovi
(Belgrade, Serbia : Engineering Society for Corrosion, 2002)
In this work is given theoretical base of methodology which, by use STM technique and corresponding STM software, offers an good conveniences for the examination of mechanism of electrode position process.
CO tolerant Pt/Ru0.7Ti0.3O2 nanocatalyst for hydrogen oxidation reaction / Pt/Ru0,7Ti0,3O2 kao nanokatalizator za oksidaciju vodonika i njegova tolerancija na CO
(Belgrade, Serbia : Engineering Society for Corrosion, 2018)
The oxidation of pure H2 and H2/CO mixture (100 ppm CO) was investigated on Pt nanocatalyst supported on Ru0.7Ti0.3O2 (Pt /Ru0.7Ti0.3O2) by linear sweep voltammetry at a rotating disc electrode in 0.1 M HClO4. The results ...
Activated titanium anodes in cathodic protection: A comparison of the characteristics of anodes prepared by sol-gel procedure and thermal decomposition / Aktivirane titanske anode u katodnoj zaštiti - poređenje karakteristika anoda dobijenih sol-gel postupkom i termičkom razgradnjom
(Belgrade, Serbia : Engineering Society for Corrosion, 2004)
Polarization characteristics of titanium anodes, coated by active RuO2-TiO2 binary oxide using sol-gel preparation procedure and chloride thermal decomposition, in oxygen evolution reaction during anode electrolytic ...
Solvatochromism of N-aryl-phenylacetamides / Solvatohromizam N-aril-fenilacetamida
(Belgrade, Serbia : Engineering Society for Corrosion, 2016)
Amide derivates are biologically active compounds and they are widely used in all spheres of life. Therefore, it is very important to know their physical-chemical properties. In this work the influence of characteristics ...
Influence of welding current intensity on pitting corrosion resistance in welded joint of stainless steel X5CrNi18-10 / Uticaj jačine struje zavarivanja na otpornost prema piting koroziji zavarenog spoja nerđajućeg čelika X5CrNi18-10
(Belgrade, Serbia : Engineering Society for Corrosion, 2017)
The effect of welding current on the pitting corrosion resistance in the welded joint of austenitic stainless steel X5CrNi18-10 was tested. Welding was carried out using three different current intensity (110 A, 130 A and ...
Chemical investigation of miscanthus × giganteus Greef et Deu. Cultivated in Serbia: A potential renewable source of energy / Hemijska ispitivanja miskantusa gajenog u Srbiji - potencijalni obnovljiv izvor energije
(Belgrade, Serbia : Engineering Society for Corrosion, 2016)
According to scientific community and professional specialists, urging necessity to increase capacity of sources of energy can be partially achieved by using biomass as a raw material. This approach is justified by both ...