Effect of mechanical-chemical activation of flotation tailings on removal the useful components
Uticaj mehano-hemijske aktivacije flotacijske jalovine na stepen izdvajanja korisnih komponenti
Abstract
The presented results refer to the investigation of effect the mechanical-chemical activation of flotation tailings on copper, iron and sulfur leaching degree in the sulfuric-chloride solution with the addition of H2O2 as oxidant. A sample of the Bor flotation tailings (BFT) from the old Bor flotation tailing dump consists of pyrite and tailings as the main components, and is activated in a dry process of the vibro mill with (BFT1) and without (BFT2) addition of NaOH as the chemical reagent. Using the dry magnetic separation in thee high-gradient magnetic separator Sala, the samples were separated into magnetic and non-magnetic fraction, BFT MF and BFT NMF, respectively. Leaching of various treated samples showed that the highest level of copper leaching (98.7 wt %), was obtained for BFJ2 MF sample while the leaching degree of Fe and S was higher in non-magnetic fractions, up to 92.46 wt % in BFT1 NMF sample for Fe and 80.62 wt % for S in BFT2 NMF sample.
Prikazani rezultati odnose se na ispitivanje uticaja mehano-hemijske aktivacije flotacijske jalovine na stepen izluženja bakra, gvožđa i sumpora u sumporno-hloridnom rastvoru uz dodatak H2O2 kao oksidansa. Uzorak borske flotacijske jalovine (BFJ) sa lokacije starog borskog flotacijskog jalovišta sadrži 23% pirita i 75,23% jalovine kao osnovne komponente, a aktiviran je suvim postupkom u vibro mlinu bez i sa dodatkom NaOH kao hemijskog reagensa, uzorci BFJ1 i BFJ2, respektivno. Suvom magnetnom separacijom u visokogradijentnom magnetnom separatoru 'Sala', uzorci su razdvojeni na magnetičnu i nemagnetičnu frakciju, BFJ MF i BFJ NMF, respektivno. Luženje različito tretiranih uzoraka pokazalo je da je najviši stepen izluženja bakra, 98,7 %, postignut kod uzorka BFJ2 MF dok je stepen izluženja Fe i S viši kod nemagnetičnih frakcija, i kreće se do 92,46 % kod uzorka BFJ1 NMF za Fe i 80,62 % za S iz uzorka BFJ2 NMF.
Keywords:
flotation tailings / mechanical-chemical activation / magnetic separation / leaching / Cu / Fe / S / flotacijska jalovina / mehano-hemijska aktivacija / magnetna separacija / luženje / Cu / Fe / SSource:
Rudarski radovi, Bor, 2010, 2, 155-166Funding / projects:
URI
https://cer.ihtm.bg.ac.rs/handle/123456789/746https://irmbor.co.rs/wp-content/uploads/2016/12/rudarski2_10.pdf
Collections
Institution/Community
IHTMTY - JOUR AU - Marković, Radmila AU - Mladenović, Ljiljana AU - Petrov, Milan AU - Stevanović, Jasmina PY - 2010 UR - https://cer.ihtm.bg.ac.rs/handle/123456789/746 UR - https://irmbor.co.rs/wp-content/uploads/2016/12/rudarski2_10.pdf AB - The presented results refer to the investigation of effect the mechanical-chemical activation of flotation tailings on copper, iron and sulfur leaching degree in the sulfuric-chloride solution with the addition of H2O2 as oxidant. A sample of the Bor flotation tailings (BFT) from the old Bor flotation tailing dump consists of pyrite and tailings as the main components, and is activated in a dry process of the vibro mill with (BFT1) and without (BFT2) addition of NaOH as the chemical reagent. Using the dry magnetic separation in thee high-gradient magnetic separator Sala, the samples were separated into magnetic and non-magnetic fraction, BFT MF and BFT NMF, respectively. Leaching of various treated samples showed that the highest level of copper leaching (98.7 wt %), was obtained for BFJ2 MF sample while the leaching degree of Fe and S was higher in non-magnetic fractions, up to 92.46 wt % in BFT1 NMF sample for Fe and 80.62 wt % for S in BFT2 NMF sample. AB - Prikazani rezultati odnose se na ispitivanje uticaja mehano-hemijske aktivacije flotacijske jalovine na stepen izluženja bakra, gvožđa i sumpora u sumporno-hloridnom rastvoru uz dodatak H2O2 kao oksidansa. Uzorak borske flotacijske jalovine (BFJ) sa lokacije starog borskog flotacijskog jalovišta sadrži 23% pirita i 75,23% jalovine kao osnovne komponente, a aktiviran je suvim postupkom u vibro mlinu bez i sa dodatkom NaOH kao hemijskog reagensa, uzorci BFJ1 i BFJ2, respektivno. Suvom magnetnom separacijom u visokogradijentnom magnetnom separatoru 'Sala', uzorci su razdvojeni na magnetičnu i nemagnetičnu frakciju, BFJ MF i BFJ NMF, respektivno. Luženje različito tretiranih uzoraka pokazalo je da je najviši stepen izluženja bakra, 98,7 %, postignut kod uzorka BFJ2 MF dok je stepen izluženja Fe i S viši kod nemagnetičnih frakcija, i kreće se do 92,46 % kod uzorka BFJ1 NMF za Fe i 80,62 % za S iz uzorka BFJ2 NMF. T2 - Rudarski radovi, Bor T1 - Effect of mechanical-chemical activation of flotation tailings on removal the useful components T1 - Uticaj mehano-hemijske aktivacije flotacijske jalovine na stepen izdvajanja korisnih komponenti IS - 2 SP - 155 EP - 166 UR - https://hdl.handle.net/21.15107/rcub_cer_746 ER -
@article{ author = "Marković, Radmila and Mladenović, Ljiljana and Petrov, Milan and Stevanović, Jasmina", year = "2010", abstract = "The presented results refer to the investigation of effect the mechanical-chemical activation of flotation tailings on copper, iron and sulfur leaching degree in the sulfuric-chloride solution with the addition of H2O2 as oxidant. A sample of the Bor flotation tailings (BFT) from the old Bor flotation tailing dump consists of pyrite and tailings as the main components, and is activated in a dry process of the vibro mill with (BFT1) and without (BFT2) addition of NaOH as the chemical reagent. Using the dry magnetic separation in thee high-gradient magnetic separator Sala, the samples were separated into magnetic and non-magnetic fraction, BFT MF and BFT NMF, respectively. Leaching of various treated samples showed that the highest level of copper leaching (98.7 wt %), was obtained for BFJ2 MF sample while the leaching degree of Fe and S was higher in non-magnetic fractions, up to 92.46 wt % in BFT1 NMF sample for Fe and 80.62 wt % for S in BFT2 NMF sample., Prikazani rezultati odnose se na ispitivanje uticaja mehano-hemijske aktivacije flotacijske jalovine na stepen izluženja bakra, gvožđa i sumpora u sumporno-hloridnom rastvoru uz dodatak H2O2 kao oksidansa. Uzorak borske flotacijske jalovine (BFJ) sa lokacije starog borskog flotacijskog jalovišta sadrži 23% pirita i 75,23% jalovine kao osnovne komponente, a aktiviran je suvim postupkom u vibro mlinu bez i sa dodatkom NaOH kao hemijskog reagensa, uzorci BFJ1 i BFJ2, respektivno. Suvom magnetnom separacijom u visokogradijentnom magnetnom separatoru 'Sala', uzorci su razdvojeni na magnetičnu i nemagnetičnu frakciju, BFJ MF i BFJ NMF, respektivno. Luženje različito tretiranih uzoraka pokazalo je da je najviši stepen izluženja bakra, 98,7 %, postignut kod uzorka BFJ2 MF dok je stepen izluženja Fe i S viši kod nemagnetičnih frakcija, i kreće se do 92,46 % kod uzorka BFJ1 NMF za Fe i 80,62 % za S iz uzorka BFJ2 NMF.", journal = "Rudarski radovi, Bor", title = "Effect of mechanical-chemical activation of flotation tailings on removal the useful components, Uticaj mehano-hemijske aktivacije flotacijske jalovine na stepen izdvajanja korisnih komponenti", number = "2", pages = "155-166", url = "https://hdl.handle.net/21.15107/rcub_cer_746" }
Marković, R., Mladenović, L., Petrov, M.,& Stevanović, J.. (2010). Effect of mechanical-chemical activation of flotation tailings on removal the useful components. in Rudarski radovi, Bor(2), 155-166. https://hdl.handle.net/21.15107/rcub_cer_746
Marković R, Mladenović L, Petrov M, Stevanović J. Effect of mechanical-chemical activation of flotation tailings on removal the useful components. in Rudarski radovi, Bor. 2010;(2):155-166. https://hdl.handle.net/21.15107/rcub_cer_746 .
Marković, Radmila, Mladenović, Ljiljana, Petrov, Milan, Stevanović, Jasmina, "Effect of mechanical-chemical activation of flotation tailings on removal the useful components" in Rudarski radovi, Bor, no. 2 (2010):155-166, https://hdl.handle.net/21.15107/rcub_cer_746 .