dc.description.abstractSolid diphenyl itaconate monomer was obtained by esterification in the presence of diphosphorus pentoxide and polymerized in bulk with AIBN as initiator. The non-film forming polymer powder was characterized by fractionation, viscosity measurements, light scattering and other techniques. The relation [n] = 3·6 × 10-3M0·70w, obtained for toluene at 25° was extrapolated to θ-conditions by various procedures: the σ-value of 2·60 for unperturbed dimensions indicates a less pronounced influence of phenyl compared with other C6 hydrocarbon substitutes.sr
dc.language.isoensr
dc.publisherElseviersr
dc.relationThe Fund of Scientific Research of the Socialist Republic of Serbiasr
dc.rightsrestrictedAccesssr
dc.sourceEuropean Polymer Journalsr
dc.subjectSynthesissr
dc.subjectproperties of poly(diphenyl itaconate)sr
dc.subjectesterificationsr
dc.subjectdiphosphorus pentoxidesr
dc.subjectpolymerizationsr
dc.subjectAIBNsr
dc.titleSynthesis and solution properties of poly(diphenyl itaconate)sr
dc.typearticlesr
dc.rights.licenseARRsr
dcterms.abstractПлавшић, Миленко Б.; Величковић, Јован С.;
dc.citation.volume12
dc.citation.issue3
dc.citation.spage151
dc.citation.epage154
dc.identifier.doi10.1016/0014-3057(76)90044-6
dc.identifier.scopus2-s2.0-17044400401
dc.type.versionpublishedVersionsr


Документи

Thumbnail

Овај документ се појављује у следећим колекцијама

Приказ основних података о документу