Solid diphenyl itaconate monomer was obtained by esterification in the presence of diphosphorus pentoxide and polymerized in bulk with AIBN as initiator. The non-film forming polymer powder was characterized by fractionation, viscosity measurements, light scattering and other techniques. The relation [n] = 3·6 × 10-3M0·70w, obtained for toluene at 25° was extrapolated to θ-conditions by various procedures: the σ-value of 2·60 for unperturbed dimensions indicates a less pronounced influence of phenyl compared with other C6 hydrocarbon substitutes.
Keywords:
Synthesis / properties of poly(diphenyl itaconate) / esterification / diphosphorus pentoxide / polymerization / AIBNSource:
European Polymer Journal, 1976, 12, 3, 151-154Publisher:
- Elsevier
Funding / projects:
- The Fund of Scientific Research of the Socialist Republic of Serbia
Collections
Institution/Community
IHTMTY - JOUR AU - Veličković, Jovan S. AU - Plavšić, Milenko B. PY - 1976 UR - https://cer.ihtm.bg.ac.rs/handle/123456789/4663 AB - Solid diphenyl itaconate monomer was obtained by esterification in the presence of diphosphorus pentoxide and polymerized in bulk with AIBN as initiator. The non-film forming polymer powder was characterized by fractionation, viscosity measurements, light scattering and other techniques. The relation [n] = 3·6 × 10-3M0·70w, obtained for toluene at 25° was extrapolated to θ-conditions by various procedures: the σ-value of 2·60 for unperturbed dimensions indicates a less pronounced influence of phenyl compared with other C6 hydrocarbon substitutes. PB - Elsevier T2 - European Polymer Journal T1 - Synthesis and solution properties of poly(diphenyl itaconate) VL - 12 IS - 3 SP - 151 EP - 154 DO - 10.1016/0014-3057(76)90044-6 ER -
@article{ author = "Veličković, Jovan S. and Plavšić, Milenko B.", year = "1976", abstract = "Solid diphenyl itaconate monomer was obtained by esterification in the presence of diphosphorus pentoxide and polymerized in bulk with AIBN as initiator. The non-film forming polymer powder was characterized by fractionation, viscosity measurements, light scattering and other techniques. The relation [n] = 3·6 × 10-3M0·70w, obtained for toluene at 25° was extrapolated to θ-conditions by various procedures: the σ-value of 2·60 for unperturbed dimensions indicates a less pronounced influence of phenyl compared with other C6 hydrocarbon substitutes.", publisher = "Elsevier", journal = "European Polymer Journal", title = "Synthesis and solution properties of poly(diphenyl itaconate)", volume = "12", number = "3", pages = "151-154", doi = "10.1016/0014-3057(76)90044-6" }
Veličković, J. S.,& Plavšić, M. B.. (1976). Synthesis and solution properties of poly(diphenyl itaconate). in European Polymer Journal Elsevier., 12(3), 151-154. https://doi.org/10.1016/0014-3057(76)90044-6
Veličković JS, Plavšić MB. Synthesis and solution properties of poly(diphenyl itaconate). in European Polymer Journal. 1976;12(3):151-154. doi:10.1016/0014-3057(76)90044-6 .
Veličković, Jovan S., Plavšić, Milenko B., "Synthesis and solution properties of poly(diphenyl itaconate)" in European Polymer Journal, 12, no. 3 (1976):151-154, https://doi.org/10.1016/0014-3057(76)90044-6 . .