Examination of the kinetics of Zr1.02Ni0.98 alloy hydriding
Ispitivanje reakcije hidriranja legure Zr1.02Ni0.98
Članak u časopisu (Objavljena verzija)
Metapodaci
Prikaz svih podataka o dokumentuApstrakt
The hydriding kinetics of Zr1.02Ni0.98 alloy was examined in dependence on the number of hydriding/dehydriding cycles. The rate constants relating to three subsequent hydriding procedures of an alloy sample, at five temperatures: 423, 448, 473, 498 and 523 K, were determined. The rate constant increases, and the activation energy decreases on each repetition of the hydriding/dehydriding cycle at a given temperature. This behavior was explained by sample crushing, leading to an increase in the surface area accessible to hydrogen.
Ispitivna je kinetika hidriranja legure Zr1.02Ni0.98 u zavisnosti od broja ciklusa
hidriranja/dehidriranja. Određene su konstante brzina za tri uzastopne reakcije hidriranja na uzorku legure, na pet temperatura: 423, 448, 473, 498 i 523 K. Ponavljanje
ciklusa hidriranja/dehidriranja praćeno je stalnim porastom konstante brzine i opadanjem aktivacione energije.Ova pojava je objašnjena usitnjavanjem uzorka,što dovodi
do povećanja površine koja je dostupna vodoniku.
Ključne reči:
Activaiton energy / Hydriding rate constant / Zirconium-nickel alloy / Hydriding/dehydriding / legura / aktivaciona energija / vodonikIzvor:
Journal of the Serbian Chemical Society, 1999, 64, 12, 745-752Izdavač:
- Belgrade : Serbian Chemical Society
Finansiranje / projekti:
- The Ministry of Sciences and Technology of the Republic of Serbia (Project No. 02E-15)
Institucija/grupa
IHTMTY - JOUR AU - Simonović, Branislav AU - Mentus, Slavko AU - Šušić, Milenko PY - 1999 UR - https://cer.ihtm.bg.ac.rs/handle/123456789/4402 AB - The hydriding kinetics of Zr1.02Ni0.98 alloy was examined in dependence on the number of hydriding/dehydriding cycles. The rate constants relating to three subsequent hydriding procedures of an alloy sample, at five temperatures: 423, 448, 473, 498 and 523 K, were determined. The rate constant increases, and the activation energy decreases on each repetition of the hydriding/dehydriding cycle at a given temperature. This behavior was explained by sample crushing, leading to an increase in the surface area accessible to hydrogen. AB - Ispitivna je kinetika hidriranja legure Zr1.02Ni0.98 u zavisnosti od broja ciklusa hidriranja/dehidriranja. Određene su konstante brzina za tri uzastopne reakcije hidriranja na uzorku legure, na pet temperatura: 423, 448, 473, 498 i 523 K. Ponavljanje ciklusa hidriranja/dehidriranja praćeno je stalnim porastom konstante brzine i opadanjem aktivacione energije.Ova pojava je objašnjena usitnjavanjem uzorka,što dovodi do povećanja površine koja je dostupna vodoniku. PB - Belgrade : Serbian Chemical Society T2 - Journal of the Serbian Chemical Society T1 - Examination of the kinetics of Zr1.02Ni0.98 alloy hydriding T1 - Ispitivanje reakcije hidriranja legure Zr1.02Ni0.98 VL - 64 IS - 12 SP - 745 EP - 752 DO - 10.2298/jsc9912745s ER -
@article{ author = "Simonović, Branislav and Mentus, Slavko and Šušić, Milenko", year = "1999", abstract = "The hydriding kinetics of Zr1.02Ni0.98 alloy was examined in dependence on the number of hydriding/dehydriding cycles. The rate constants relating to three subsequent hydriding procedures of an alloy sample, at five temperatures: 423, 448, 473, 498 and 523 K, were determined. The rate constant increases, and the activation energy decreases on each repetition of the hydriding/dehydriding cycle at a given temperature. This behavior was explained by sample crushing, leading to an increase in the surface area accessible to hydrogen., Ispitivna je kinetika hidriranja legure Zr1.02Ni0.98 u zavisnosti od broja ciklusa hidriranja/dehidriranja. Određene su konstante brzina za tri uzastopne reakcije hidriranja na uzorku legure, na pet temperatura: 423, 448, 473, 498 i 523 K. Ponavljanje ciklusa hidriranja/dehidriranja praćeno je stalnim porastom konstante brzine i opadanjem aktivacione energije.Ova pojava je objašnjena usitnjavanjem uzorka,što dovodi do povećanja površine koja je dostupna vodoniku.", publisher = "Belgrade : Serbian Chemical Society", journal = "Journal of the Serbian Chemical Society", title = "Examination of the kinetics of Zr1.02Ni0.98 alloy hydriding, Ispitivanje reakcije hidriranja legure Zr1.02Ni0.98", volume = "64", number = "12", pages = "745-752", doi = "10.2298/jsc9912745s" }
Simonović, B., Mentus, S.,& Šušić, M.. (1999). Examination of the kinetics of Zr1.02Ni0.98 alloy hydriding. in Journal of the Serbian Chemical Society Belgrade : Serbian Chemical Society., 64(12), 745-752. https://doi.org/10.2298/jsc9912745s
Simonović B, Mentus S, Šušić M. Examination of the kinetics of Zr1.02Ni0.98 alloy hydriding. in Journal of the Serbian Chemical Society. 1999;64(12):745-752. doi:10.2298/jsc9912745s .
Simonović, Branislav, Mentus, Slavko, Šušić, Milenko, "Examination of the kinetics of Zr1.02Ni0.98 alloy hydriding" in Journal of the Serbian Chemical Society, 64, no. 12 (1999):745-752, https://doi.org/10.2298/jsc9912745s . .