Приказ основних података о документу

Stvarna površina eletrode od aluminijuma u rastvoru natrijum-hlorida

dc.creatorDražić, Dragutin M.
dc.creatorPopić, Jovan P.
dc.creatorRakočević, Zlatko Lj.
dc.date.accessioned2021-03-26T15:12:33Z
dc.date.available2021-03-26T15:12:33Z
dc.date.issued1999
dc.identifier.issn0352-5139
dc.identifier.issn1820-7421
dc.identifier.urihttps://cer.ihtm.bg.ac.rs/handle/123456789/4397
dc.description.abstractBy combining the techniques of electrochemical slow potentiodynamic, AC impedance and atomic force microscopy (AFM), it was shown that the differences in the anodic dissolution rates of Al in 0.5 NaCl solutions as measured experimentally in the potential region between the corrosion and pitting potential, are mainly due to differences in surface roughness of the electrodes used. It was shown that mechanical grinding and polishing of the electrode surface with emery paper (400 grit) and alumina polishing powder ((Latin small letter o with stroke) 0.25 μm) can produce surfaces differing by a factor of 6 in the roughness factor Ra. By using AFM estimates of the roughness factors a true electrode capacitance of 4.63 μC cm-2 and thickness dox ≈ 2.0 nm for the barrier layer of the surface film was estamited. The outer part of the film is porous, partly as amorphous A1(OH)3, or crystalline bayerite (Al2O3-3H2O).sr
dc.description.abstractPokazano je, kombinovanim korišćenjem tehnika spore potenciodinamike, AC impedance i atomske mikroskopije (AFM), da su razlike u brzinama anodnog rastvarača Al u 0,5 M NaCl u oblasti između korozionog i piting potencijala, a koje se zapažaju u eksperimentima, prvenstveno posledica razlike u površinskoj hrapavosti različito pripremljenih elektroda. Pokazano je da se mehaničkim brušenjem (finoća 400) i poliranjem Al2O3 pastom (0,25 mm) dobija razlika faktora hrapavosti za oko 6 puta. Uz pomoć AFM tehnike za određivanje faktora hrapavosti procenjena je prava kapacitivnost elektroda od 4,63 mF cm–2 i debljina barijernog sloja oksida od dox ≈ 2,0 nm. Spoljašnji porozni sloj je delimično amorfan Al(OH)3 ili kristalinični bajerit (Al2O3.3H2O).sr
dc.language.isoensr
dc.publisherBelgrade : Serbian Chemical Societysr
dc.relationThe Ministry of Science and Technology of Serbiasr
dc.rightsopenAccesssr
dc.rights.urihttps://creativecommons.org/licenses/by-nc-nd/4.0/
dc.sourceJournal of the Serbian Chemical Societysr
dc.subjectaluminiumsr
dc.subjectCorrosionsr
dc.subjectreal surface areasr
dc.subjectoxide thicknesssr
dc.titleReal surface area of the aluminium electrode in sodium chloride solutionsr
dc.titleStvarna površina eletrode od aluminijuma u rastvoru natrijum-hloridasr
dc.typearticlesr
dc.rights.licenseBY-NC-NDsr
dcterms.abstractДражић, Драгутин М.; Ракочевић, Златко Љ.; Попић, Јован П.; Стварна површина елетроде од алуминијума у раствору натријум-хлорида; Стварна површина елетроде од алуминијума у раствору натријум-хлорида;
dc.citation.volume64
dc.citation.issue11
dc.citation.spage685
dc.citation.epage685
dc.identifier.doi10.2298/jsc9911685d
dc.identifier.fulltexthttps://cer.ihtm.bg.ac.rs/bitstream/id/19676/bitstream_19676.pdf