dc.creatorĆosović, Vladan
dc.creatorGrujić, Aleksandar
dc.creatorStajić-Trošić, Jasna
dc.creatorSpasojević, Vojislav
dc.creatorTalijan, Nadežda M.
dc.date.accessioned2019-01-30T17:16:14Z
dc.date.available2019-01-30T17:16:14Z
dc.date.issued2007
dc.identifier.issn0255-5476
dc.identifier.urihttps://cer.ihtm.bg.ac.rs/handle/123456789/345
dc.description.abstractPhase transformations and magnetic properties of multiphase Nd 4.5Fe76.2B19.5 alloy were investigated in the temperature range of heat treatment 600-700°C. The influence of different heat treatment regimes was observed by correlation of phase composition and measured magnetic properties. The heat treatment regime, which provided the microstructure that improves exchange interactions between grains of soft and hard magnetic phases and consequently enhances magnetic properties, was defined and discussed. For optimized magnetic alloy grain size of the present phases Fe3B, Nd2Fe14B and α-Fe was calculated by size-strain analysis of X-ray powder diffraction data. Calculated mean grain size was on a nanoscale, below 30 nm.en
dc.relationinfo:eu-repo/grantAgreement/MESTD/MPN2006-2010/142035/RS//
dc.rightsrestrictedAccess
dc.sourceMaterials Science Forum
dc.subjectHeat treatmenten
dc.subjectInteractive intergranular mechanismen
dc.subjectMagnetic propertiesen
dc.subjectNanocompositeen
dc.subjectPhase compositionen
dc.titlePhase composition and magnetic properties of multiphase melt-spun Nd 4.3Fe76.2B19.5alloyen
dc.typeconferenceObject
dc.rights.licenseARR
dcterms.abstractЋосовић, Владан; Спасојевић, В.; Стајић Трошић, Јасна; Грујић, Aлександар; Талијан, Надежда М.;
dc.citation.volume555
dc.citation.spage527
dc.citation.epage532
dc.citation.other555: 527-532
dc.citation.rankM23
dc.identifier.doi10.4028/www.scientific.net/MSF.555.527