Characterization and corrosion properties of electrodeposited Ni-W alloys / Karakterizacija i korozione karakteristike elektrohemijski taložene legure Ni-W
(Serbian Chemical Society, 2001)
Ni-W alloys electrodeposited from citrate solution consist of three different phases, which are all present in high W-content alloys: a solid solution of W in a Ni matrix; an intermetallic compound Ni4W, as well as another ...
Corrosion potential of 304 stainless steel in sulfuric acid / Korozioni potencijal nerđajućeg čelika 304 u sumpornoj kiselini
(Serbian Chemical Society, 2006)
The potentiodynamic study of the electrochemical behavior of austenitic 304 stainless steel in deaerated aqueous sulfuric acid of pH 1 revealed that the steel achieved a stable corrosion potential of ca. - 0.350 V (SCE) ...
Influence of chloride ions on the open circuit potentials of chromium in deaerated sulfuric acid solutions / Uticaj hloridnih jona na potencijal otvorenog kola hroma u deaerisanim rastvorima sumporne kiseline
(Serbian Chemical Society, 2006)
Open circuit potential measurements and cyclic voltammetry of chromium in deaerated aqueous H2SO4 solution of pH 1 without and containing NaCl in the concentration range 0.5 - 4 M revealed that chromium exhibits two stable ...
Corrosion causes in thermal power plants and ways of prevention / Uzroci korozije u termoenergetskim postrojenjima i načini prevencije
(Belgrade, Serbia : Engineering Society for Corrosion, 2009)
Corrosion damages often exert considerable influence on outages number and hence on the loss of thermal power plant availability. In order to accomplish the aim of reducing the corrosion to it's minimum and prevent main ...
Structural effects of metallic chromium on its electrochemical behavior / Uticaj strukture metalnog hroma na njegovo elektrohemijsko ponašanje
(Serbian Chemical Society, 2007)
Chromium dissolution in aqueous sulfuric acid solution of pH 1 was studied electrochemically on chromium electrodes with different crystallographic structures. A slow potentiodynamic method was used for the electrochemical ...
Magneto electrochemistry: Basic facts and the effects of the applied magnetic fields onto corrosion of metals, mass transfers, kinetic of process and the preferred orientation of deposits / Magneto-elektrohemija - osnovne činjenice i uticaji primenjenog magnetnog polja na koroziju metala, prenos mase, kinetiku procesa i preferencijalnu orijentaciju taloga
(Belgrade, Serbia : Engineering Society for Corrosion, 2005)
In this work, the theoretical survey of the basic facts about magneto electrochemistry will be given. It will be analyzed the effects of the applied magnetic fields on kinetic of the electrochemical processes, mass transfer ...
Zn-Co-CeO2 vs. Zn-Co Coatings: Effect of CeO2 Sol in the Enhancement of the Corrosion Performance of Electrodeposited Composite Coatings
(MDPI, 2021)
Electrodeposition and characterization of novel ceria-doped Zn-Co composite coatings was
the main goal of this research. Electrodeposited composite coatings were compared to pure Zn-Co
coatings obtained under the same ...
Ternary Zn-Ni-Co alloy: anomalous codeposition and corrosion stability
(Serbian Chemical Society, 2015)
Electrochemically deposited Zn-Ni-Co alloys under various deposition conditions were investigated using atomic absorption spectroscopy for the determination of the chemical composition, atomic force microscopy for surface ...
Mechanisms of hydrogen evolution on chromium / Mehanizmi izdvajanja vodonika na hromu
(Institut za rudarstvo i metalurgiju Bor, 2015)
In this work, the mechanisms of hydrogen evolution on the metal chromium in a solution of 0.1 M Na2SO4 + H2SO4, pH 1 to pH 7 were analysed. In the pH LT 3 range, hydrogen is evolved according to three different mechanisms, ...
Corrosion properties of an aluminium alloy 7000 series after a new two step precipitation hardening / Otpornost prema koroziji aluminijumske legure serije 7000 posle novog dvostepenog termičkog taloženja
(Belgrade, Serbia : Engineering Society for Corrosion, 2014)
Corrosion properties of an aluminium alloy 7000 series were investigated by different electrochemical methods. The alloy was subjected to the one-step and to a new two-step precipitation hardening. Polarization measurements ...