Effect of Tb3+ doping on the photocatalytic activity of TiO2 coatings formed by plasma electrolytic oxidation of titanium
(Elsevier, 2018)
Tb doped TiO2 coatings are formed by plasma electrolytic oxidation (PEO) of titanium in water solution of 10 g/L Na3PO4.12H(2)O with addition of Tb4O7 powder. Surface morphology, chemical, and phase composition of obtained ...
MgO/ZnO coatings formed on magnesium alloy AZ31 by plasma electrolytic oxidation: Structural, photoluminescence and photocatalytic investigation
(Elsevier, 2017)
This paper presents the results of our recent investigation of MgO/ZnO coatings formed on AZ31 magnesium alloy by plasma electrolytic oxidation in phosphate-based alkaline electrolyte with varying concentration of ZnO ...
Preparation and photocatalyic properties of TiO2-P25 film prepared by spray pyrolysis method
(Elsevier, 2013)
TiO2 films were synthesized by immobilization of Degussa P25 powders on stainless steel support by spray pyrolysis technique. After preparation, the films were annealed at different temperatures in order to obtain materials ...
Structure-activity relationship of nanosized porous PEG-modified TiO2 powders in degradation of organic pollutants
(Elsevier, 2015)
This study aims to gain insights in structure-activity relationship of TiO2 photocatalysts. For this purpose photocatalysts were synthesized via classical sol-gel method using titanium isopropoxide as a precursor and ...
CdS particles modified TiO2 coatings formed by plasma electrolytic oxidation with enhanced photocatalytic activity
(Elsevier, 2018)
CdS particles modified anatase TiO2 photocatalysts were formed on titanium substrate by plasma electrolytic oxidation for 2 min in supporting electrolyte (10 g/L Na-3 center dot PO4 center dot 12H(2)O) with addition of CdS ...
TiO2/WO3 photocatalytic composite coatings prepared by spray pyrolysis
(Elsevier, 2014)
TiO2/WO3 composites supported on a stainless steel foil were prepared by the spray pyrolysis technique. Content of WO3 was gradually increased from 1 wt% to 100 wt.%, while the coating thickness was limited to about 1 pm. ...