Anaphoretical/oxidative approach to the in-situ synthesis of adherent hydroxyapatite/titanium oxide composite coatings on titanium
(Elsevier, 2019)
In-situ synthesis of HAp/TiO2 coating on titanium was performed via anaphoretic deposition of HAp and simultaneous anodization of Ti to produce highly adherent and strengthened composite coating. The prepared coatings were ...
Deposition of silver ions onto DBD and DCSBD plasma treated nonwoven polypropylene
(Elsevier, 2012)
The aim of this work is plasma activation of nonwoven polypropylene (PP) using two different ambient air plasma sources: volume dielectric barrier discharge (DBD) and diffuse coplanar surface barrier discharge (DCSBD) and ...
CdS particles modified TiO2 coatings formed by plasma electrolytic oxidation with enhanced photocatalytic activity
(Elsevier, 2018)
CdS particles modified anatase TiO2 photocatalysts were formed on titanium substrate by plasma electrolytic oxidation for 2 min in supporting electrolyte (10 g/L Na-3 center dot PO4 center dot 12H(2)O) with addition of CdS ...
Anaphoretical/oxidative approach to the in-situ synthesis of adherent hydroxyapatite/titanium oxide composite coatings on titanium
(Elsevier, 2019)
In-situ synthesis of HAp/TiO2 coating on titanium was performed via anaphoretic deposition of HAp and simultaneous anodization of Ti to produce highly adherent and strengthened composite coating. The prepared coatings were ...
CdS particles modified TiO2 coatings formed by plasma electrolytic oxidation with enhanced photocatalytic activity
(Elsevier, 2018)
CdS particles modified anatase TiO2 photocatalysts were formed on titanium substrate by plasma electrolytic oxidation for 2 min in supporting electrolyte (10 g/L Na-3 center dot PO4 center dot 12H(2)O) with addition of CdS ...
TiO2/WO3 photocatalytic composite coatings prepared by spray pyrolysis
(Elsevier, 2014)
TiO2/WO3 composites supported on a stainless steel foil were prepared by the spray pyrolysis technique. Content of WO3 was gradually increased from 1 wt% to 100 wt.%, while the coating thickness was limited to about 1 pm. ...