Effect of mechanical-chemical activation of flotation tailings on removal the useful components

Marković, Radmila; Mladenović, Ljiljana; Petrov, Milan; Stevanović, Jasmina

(2010)

TY  - JOUR
AU  - Marković, Radmila
AU  - Mladenović, Ljiljana
AU  - Petrov, Milan
AU  - Stevanović, Jasmina
PY  - 2010
UR  - https://cer.ihtm.bg.ac.rs/handle/123456789/746
UR  - https://irmbor.co.rs/wp-content/uploads/2016/12/rudarski2_10.pdf
AB  - The presented results refer to the investigation of effect the mechanical-chemical activation of flotation tailings on copper, iron and sulfur leaching degree in the sulfuric-chloride solution with the addition of H2O2 as oxidant. A sample of the Bor flotation tailings (BFT) from the old Bor flotation tailing dump consists of pyrite and tailings as the main components, and is activated in a dry process of the vibro mill with (BFT1) and without (BFT2) addition of NaOH as the chemical reagent. Using the dry magnetic separation in thee high-gradient magnetic separator Sala, the samples were separated into magnetic and non-magnetic fraction, BFT MF and BFT NMF, respectively. Leaching of various treated samples showed that the highest level of copper leaching (98.7 wt %), was obtained for BFJ2 MF sample while the leaching degree of Fe and S was higher in non-magnetic fractions, up to 92.46 wt % in BFT1 NMF sample for Fe and 80.62 wt % for S in BFT2 NMF sample.
AB  - Prikazani rezultati odnose se na ispitivanje uticaja mehano-hemijske aktivacije flotacijske jalovine na stepen izluženja bakra, gvožđa i sumpora u sumporno-hloridnom rastvoru uz dodatak H2O2 kao oksidansa. Uzorak borske flotacijske jalovine (BFJ) sa lokacije starog borskog flotacijskog jalovišta sadrži 23% pirita i 75,23% jalovine kao osnovne komponente, a aktiviran je suvim postupkom u vibro mlinu bez i sa dodatkom NaOH kao hemijskog reagensa, uzorci BFJ1 i BFJ2, respektivno. Suvom magnetnom separacijom u visokogradijentnom magnetnom separatoru 'Sala', uzorci su razdvojeni na magnetičnu i nemagnetičnu frakciju, BFJ MF i BFJ NMF, respektivno. Luženje različito tretiranih uzoraka pokazalo je da je najviši stepen izluženja bakra, 98,7 %, postignut kod uzorka BFJ2 MF dok je stepen izluženja Fe i S viši kod nemagnetičnih frakcija, i kreće se do 92,46 % kod uzorka BFJ1 NMF za Fe i 80,62 % za S iz uzorka BFJ2 NMF.
T2  - Rudarski radovi, Bor
T1  - Effect of mechanical-chemical activation of flotation tailings on removal the useful components
T1  - Uticaj mehano-hemijske aktivacije flotacijske jalovine na stepen izdvajanja korisnih komponenti
IS  - 2
SP  - 155
EP  - 166
UR  - https://hdl.handle.net/21.15107/rcub_cer_746
ER  - 
@article{
author = "Marković, Radmila and Mladenović, Ljiljana and Petrov, Milan and Stevanović, Jasmina",
year = "2010",
abstract = "The presented results refer to the investigation of effect the mechanical-chemical activation of flotation tailings on copper, iron and sulfur leaching degree in the sulfuric-chloride solution with the addition of H2O2 as oxidant. A sample of the Bor flotation tailings (BFT) from the old Bor flotation tailing dump consists of pyrite and tailings as the main components, and is activated in a dry process of the vibro mill with (BFT1) and without (BFT2) addition of NaOH as the chemical reagent. Using the dry magnetic separation in thee high-gradient magnetic separator Sala, the samples were separated into magnetic and non-magnetic fraction, BFT MF and BFT NMF, respectively. Leaching of various treated samples showed that the highest level of copper leaching (98.7 wt %), was obtained for BFJ2 MF sample while the leaching degree of Fe and S was higher in non-magnetic fractions, up to 92.46 wt % in BFT1 NMF sample for Fe and 80.62 wt % for S in BFT2 NMF sample., Prikazani rezultati odnose se na ispitivanje uticaja mehano-hemijske aktivacije flotacijske jalovine na stepen izluženja bakra, gvožđa i sumpora u sumporno-hloridnom rastvoru uz dodatak H2O2 kao oksidansa. Uzorak borske flotacijske jalovine (BFJ) sa lokacije starog borskog flotacijskog jalovišta sadrži 23% pirita i 75,23% jalovine kao osnovne komponente, a aktiviran je suvim postupkom u vibro mlinu bez i sa dodatkom NaOH kao hemijskog reagensa, uzorci BFJ1 i BFJ2, respektivno. Suvom magnetnom separacijom u visokogradijentnom magnetnom separatoru 'Sala', uzorci su razdvojeni na magnetičnu i nemagnetičnu frakciju, BFJ MF i BFJ NMF, respektivno. Luženje različito tretiranih uzoraka pokazalo je da je najviši stepen izluženja bakra, 98,7 %, postignut kod uzorka BFJ2 MF dok je stepen izluženja Fe i S viši kod nemagnetičnih frakcija, i kreće se do 92,46 % kod uzorka BFJ1 NMF za Fe i 80,62 % za S iz uzorka BFJ2 NMF.",
journal = "Rudarski radovi, Bor",
title = "Effect of mechanical-chemical activation of flotation tailings on removal the useful components, Uticaj mehano-hemijske aktivacije flotacijske jalovine na stepen izdvajanja korisnih komponenti",
number = "2",
pages = "155-166",
url = "https://hdl.handle.net/21.15107/rcub_cer_746"
}
Marković, R., Mladenović, L., Petrov, M.,& Stevanović, J.. (2010). Effect of mechanical-chemical activation of flotation tailings on removal the useful components. in Rudarski radovi, Bor(2), 155-166.
https://hdl.handle.net/21.15107/rcub_cer_746
Marković R, Mladenović L, Petrov M, Stevanović J. Effect of mechanical-chemical activation of flotation tailings on removal the useful components. in Rudarski radovi, Bor. 2010;(2):155-166.
https://hdl.handle.net/21.15107/rcub_cer_746 .
Marković, Radmila, Mladenović, Ljiljana, Petrov, Milan, Stevanović, Jasmina, "Effect of mechanical-chemical activation of flotation tailings on removal the useful components" in Rudarski radovi, Bor, no. 2 (2010):155-166,
https://hdl.handle.net/21.15107/rcub_cer_746 .