dc.description.abstractThe critical overpotential for zinc dendrite growth is determined as 173 mV by the method described by Popov et al. [1]. It was shown that this procedure can be applied successfully to metal deposition processes when there is a large codeposition of hydrogen. © 1979 Chapman and Hall Ltd.en
dc.publisherKluwer Academic Publishers
dc.rightsrestrictedAccess
dc.sourceJournal of Applied Electrochemistry
dc.subjectMetal Deposition
dc.subjectElectrochemistry
dc.titleThe critical overpotential for zinc dendrite formationen
dc.typearticleen
dc.rights.licenseARR
dcterms.abstractСпасојевић, М. Д.; Попов, К. И.; Накић, В М; Павловић, М. Г.;
dc.rights.holderChapman and Hall Ltd. 1979
dc.citation.volume9
dc.citation.issue4
dc.citation.spage533
dc.citation.epage536
dc.identifier.doi10.1007/BF00617566
dc.identifier.scopus2-s2.0-34250273749
dc.type.versionpublishedVersion


Документи

Thumbnail

Овај документ се појављује у следећим колекцијама

Приказ основних података о документу