Претраживање
Приказ резултата 1-6 од 6
Oxygen reduction on Au (100) and vicinal Au (910) and Au (11, 1, 1) faces in alkaline solution. A rotating disc-ring study
(Elsevier, 1992)
The kinetics of oxygen reduction have been studied on Au (100) and vicinal Au (910) and Au (11, 1, 1) faces in 0.1 M NaOH by a rotating disc-ring method. A very high activity of these surfaces for O2 reduction was demonstrated. ...
The roles of the ruthenium concentration profile, the stabilizing component and the substrate on the stability of oxide coatings
(Elsevier, 1992)
Electrocatalytic oxide coatings with variable concentration profiles of RuO2 as the active component were obtained through a combination of separately applied layers of RuO2, TiO2, IrO2, RuO2 + TiO2 and RuO2 + IrO2 on ...
Hydrogen adsorption on single-crystal platinum electrodes in alkaline solutions
(Elsevier, 1992)
Hydrogen adsorption on single-crystal platinum low-index and stepped surfaces was studied in 0.1 M and 0.01 M NaOH solutions. A strong dependence on the crystallographic orientation of the electrode surface was found. The ...
Oscillatory phenomena in oxygen and hydrogen peroxide reduction on the Au(100) electrode surface in alkaline solutions
(Elsevier, 1992)
In this work we report preliminary data for oscillatory behavior found in oxygen and hydrogen peroxide reduction on a rotating gold electrode with (100) orientation in alkaline solutions.
Anodic stability and electrochromism of electrodeposited ruthenium-iridium coatings on titanium
(Elsevier, 1992)
The anodic behaviour of galvanically plated ruthenium-iridium coatings on titanium was investigated. The dependence of the Tafel slopes and the stability of the coatings for the oxygen evolution reaction in sulphuric acid ...
Oxidation of d-glucose on single-crystal platinum electrodes: A mechanistic study
(Elsevier, 1992)
Reaction kinetics of glucose oxidation on single-crystal platinum electrodes has a pronounced structure sensitivity. Quasi-steady-state measurements show Tafel slopes of 120 mV per decade for Pt(111), but 60 mV per decade ...